[1]陆怡,卫渊钊,魏安安,等.焦炭塔的失效原因分析及延寿技术研究进展[J].常州大学学报(自然科学版),2022,34(02):1-7.[doi:10.3969/j.issn.2095-0411.2022.02.001]
 LU Yi,WEI Yuanzhao,WEI An'an,et al.Analysis of Causes of Failure of Coke Drums and Latest Development of Research on Life Extension Technology[J].Journal of Changzhou University(Natural Science Edition),2022,34(02):1-7.[doi:10.3969/j.issn.2095-0411.2022.02.001]
点击复制

焦炭塔的失效原因分析及延寿技术研究进展()
分享到:

常州大学学报(自然科学版)[ISSN:2095-0411/CN:32-1822/N]

卷:
第34卷
期数:
2022年02期
页码:
1-7
栏目:
化学化工
出版日期:
2022-03-28

文章信息/Info

Title:
Analysis of Causes of Failure of Coke Drums and Latest Development of Research on Life Extension Technology
文章编号:
2095-0411(2022)02-0001-07
作者:
陆怡卫渊钊魏安安刘犇欢甘刘意王园春
(常州大学机械与轨道交通学院,江苏常州213164)
Author(s):
LU Yi WEI Yuanzhao WEI An'an LIU Benhuan GAN Liuyi WANG Yuanchun
(School of Mechanical Engineering and Rail Transit, Changzhou University, Changzhou 213164, China)
关键词:
焦炭塔 失效形式 失效原因 延寿技术
Keywords:
coke drums failure mode failure reason life extension technology
分类号:
TQ 053
DOI:
10.3969/j.issn.2095-0411.2022.02.001
文献标志码:
A
摘要:
焦炭塔在生焦过程中要反复承受油气的温度、 操作压力的周期性变化及除焦时冷水冲击引起的温度变化, 致使焦炭塔在使用一定时间后会发生开裂、 鼓胀、 变形等形式的失效和损伤。研究焦炭塔的失效原因, 并对其损伤程度进行评估, 以便保障焦炭塔的长周期安全运行是多年来人们的研究目标。文章汇总了焦炭塔壳体与裙座连接部位的开裂、 壳体鼓胀变形、 壳体的倾斜变形、 焦炭塔下塔盖变形4种主要失效形式的原因以及焦炭塔延寿技术方面的研究成果, 并根据本研究团队的最新研究成果进行了分析与评述, 提出了新的失效原因, 以便为相关研究者和用户在解决工程问题时提供参考。
Abstract:
The coke tower has to repeatedly bear the cyclical changes in the temperature of the oil and gas, the operating pressure and the temperature change caused by the impact of cold water during decoking during the coking process, causing the coke tower to crack, bulge, deform and other forms of failure after a certain period of use and damage. To study the causes of the failure of the coke drum and evaluate its damage to ensure the long-term safe operation of the coke drum has been a research goal for many years. This article summarizes the four main failure causes of the joints of the coke drum shell and the skirt, the swelling deformation of the tower body, the tilting deformation of the tower body, and the deformation of the lower cover of the coke tower, as well as the research results of the coke tower life extension technology. The recent research results of the research team have been analyzed and reviewed, and new failure causes have been pointed out in order to provide references for related researchers and users when solving engineering problems.

参考文献/References:

[1]SUÁREZ-RUIZ I, DIEZ M A, RUBIERA F. Coal[M]//New Trends in Coal Conversion. Amsterdam: Elsevier, 2019: 1-30.
[2]吴娜. 焦炭塔循环载荷下的疲劳分析[D]. 北京: 中国石油大学, 2009.
[3]PENSO J, TSAI C L, HOWDEN D G, et al. Assessing deterioration conditions in coke drums[J]. Welding Journal, 2000, 79(8): 45-52.
[4]刘人怀, 宁志华. 焦炭塔鼓胀与开裂变形机理及疲劳断裂寿命预测的研究进展[J]. 压力容器, 2007, 24(2): 1-8.
[5]SATAPATHY A K. Thermal analysis of an infinite slab during quenching[J]. Communications in Numerical Methods in Engineering, 2000, 16(8): 529-536.
[6]YAN Z, ZHANG Y X, CHEN J, et al. Statistical method for the fatigue life estimation of coke drums[J]. Engineering Failure Analysis, 2015, 48: 259-271.
[7]CHEN J, XIA Z H. Fatigue behaviour of coke drum materials under thermal-mechanical cyclic loading[J]. Theoretical and Applied Mechanics Letters, 2014, 4(4): 41006.
[8]DONG J H, GUO L L, GAO B J. A finite element analysis of the cyclic plasticity behavior of circumferential weld of coke drum under moving axial temperature gradient[J]. Procedia Engineering, 2015, 130: 307-321.
[9]GONZÁLEZ J L, GÓMEZ S, GÓMEZ G. Analysis of the mechanical behavior of a delayed coker drum with a circumferentially cracked skirt[J]. Procedia Structural Integrity, 2017, 3: 33-40.
[10]张绍良, 任明皓, 卜华全. 大型Cr-Mo钢焦炭塔焊接返修技术[J]. 压力容器, 2018, 35(2): 59-65.
[11]刘在康, 柴斌斌, 何通东. 某延迟焦化装置中焦炭塔的裙座裂纹原因分析[J]. 特种设备安全技术, 2018(5): 22-25.
[12]彭蕾. 焦炭塔裙座角焊缝开裂失效分析与处理[J]. 石油化工设备技术, 2007, 28(5): 54-55.
[13]高琪, 张亚新. 焦炭塔筒体和裙座连接部位热力耦合分析[J]. 中国石油和化工标准与质量, 2013, 34(5): 35.
[14]张绍良, 梁文彬, 张韶伟, 等. 焦炭塔安全性分析研究进度与展望[J]. 石油化工设备, 2018, 47(2): 38-45.
[15]CHEN J, YAMAMOTO T, XIA Z H, et al. Experimental evaluation of fatigue life of coke drum materials with weld sections[C]. Paris: [s.n.], 2014.
[16]王清栋. 在用15CrMoR焦炭塔定期检验探究[J]. 设备管理与维修, 2017(12): 115-117.
[17]PENSO A J. Fundamental study of failure mechanisms of pressure vessels under thermo-mechanical cycling in multiphase environments[D]. Columbus: The Ohio State University, 2001.
[18]BOSWELL R S, FERRARO T. Remain life evaluation of cokedrums, plant engineering,operations,design and reliability symposium[C]. Houston: Energy Engineering Conference, 1997.
[19]DUNHAM C, CLARK R. Laser mapping of coke drums-what has been learned[C]. Louisiana: Alche Spring National Meeting, 1998.
[20]ELLIS P J, HARDIN E E. How petroleum delayed coke forms in a drum[C]. California:The Minerals,Metals and Materials Society, 1992.
[21]曹福东. 焦炭塔膨胀变形评定[J]. 中小企业管理与科技, 2009(30): 210.
[22]柳发. 焦炭塔的失效形式分析及其防范措施研究[D]. 广州: 华南理工大学, 2015.
[23]JU F, AUMULLER J, XIA Z H, et al. Global and local elastic-plastic stress analysis of coke drum under thermal-mechanical loadings[J]. Journal of Pressure Vessel Technology, 2011, 133(6): 61202.
[24]李正亮. 焦炭塔周期性倾斜对塔体和管线的安全影响评估及其治理[D]. 上海: 华东理工大学, 2017.
[25]惠志全, 林金梅, 王恋, 等. 焦炭塔定期检验案例分析[J]. 石油和化工设备, 2019, 22(11): 72-74.
[26]张玉福, 靳艳, 金铭. 焦炭塔锥体母材裂纹产生原因分析及预防措施[J]. 当代化工, 2013, 42(8): 1078-1080, 1133.
[27]陈明健, 张伟, 杨吉梅. 焦炭塔铬钼钢过渡段焊接裂纹分析[J]. 中国设备工程, 2015(8): 61-63.
[28]陈晓玲, 段滋华, 李多民. 国内外焦炭塔的研究现状及其进展[J]. 化工机械, 2009, 36(1): 56-59.
[29]刘猛, 邢爽, 尤洪川. 焦炭塔裙座裂纹分析[J]. 中小企业管理与科技, 2014(6): 314-315.
[30]侍毅. 焦炭塔裙座环焊缝裂纹原因分析及改进措施[J]. 化工机械, 2020, 47(2): 263-265.
[31]沈阳. 焦炭塔复合板裂纹原因分析及修复工艺[J]. 石油化工建设, 2012, 34(6): 76-78.
[32]周红兰. 焦炭塔裙座焊缝开裂原因分析及修复[J]. 科技创业家, 2013(20): 143.
[33]杨富明, 唐嗣伟, 赵岩, 等. 低循环比条件下的延迟焦化技术分析[J]. 石油炼制与化工, 2013, 44(4): 24-28.
[34]龚传波, 涂连涛, 张宗有, 等. 延迟焦化外甩循环油降低循环比的可行性分析[J]. 石油炼制与化工, 2017, 48(11): 60-63.
[35]刘艳, 靳松, 李金. 延迟焦化装置焦炭塔大吹汽节能研究及应用[J]. 化工管理, 2020(16): 48-49.
[36]赵岩, 王志刚, 奕龙, 等. 以水代汽工艺在延迟焦化装置上的应用[J]. 石化技术与应用, 2016, 34(5): 403-405, 427.
[37]孙世连. 延迟焦化装置焦炭塔大吹汽节能研究及应用[J]. 石化技术, 2016, 23(2): 35, 64.

备注/Memo

备注/Memo:
收稿日期: 2021-11-31。
基金项目: 江苏省研究生科研与实践创新计划资助项目(SJCX20_1002)。
作者简介: 陆怡(1973—), 女, 上海人, 硕士, 教授。 E-mail: luyi@cczu.edu.cn